Has anyone tried to repair delaminated areas of a WC-CoCr coating?
Seems like in all the forums, the only solution is to strip the whole part and recoat it.
Can you share experiences if you have tried to repair? What are the limiting principles that make so difficult to spray over a coated surface (not grinded)? Residual stresses? Clealiness?
Do you consider this a topic to develop research on? Will it be of interest? The application I have in mind is WC-CoCr for hydraulic turbines. They get delaminations in small areas.
Your input is appreciatted.
Reply
03-12-2018, 08:33 PM,
#2
RE: Repairing of delaminated areas of a WC-CoCr coating
Dear Dr. Valarezo,
Yes, it is possible with HVAF technology.
You may contact me for the details.
Regards,
Vig
Reply




Possibly Related Threads…
Thread Author Replies Views Last Post
Video Problem WC CoCr Lyokha ibn Ivanovich 2 2,527 05-24-2020, 06:13 AM
Last Post: Lyokha ibn Ivanovich
  Matrix cohesion problem of WC CoCr sams5313 2 2,425 09-22-2019, 04:34 PM
Last Post: loriolo
  Matrix cohesion problem of WC CoCr bsjkiller 0 2,297 02-22-2018, 02:08 AM
Last Post: bsjkiller
  repairing slurry pumps sutech 1 4,531 09-23-2008, 09:26 PM
Last Post: TurbineRepair
  Oxide and porosity in WC-CoCr coating ycwbycwb 4 12,482 05-10-2008, 02:39 PM
Last Post: Gordon



Users browsing this thread: 1 Guest(s)





Surface Engineering Forum Sponsor - Alphatek Hyperformance Coatings Ltd